Trust The Dynaburr Mechanical Plating Difference
At Dynaburr, our mechanical plating and galvanizing process sets the industry standard for durability, precision, and cost-efficiency. Unlike traditional electroplating or hot-dip and dip-spin methods, our advanced technology delivers superior performance for high-strength and hardened parts, ensuring exceptional corrosion resistance and uniform coatings without the drawbacks of hydrogen embrittlement or costly post-processing. The chart below outlines the clear advantages of Dynaburr’s mechanical plating, demonstrating why it’s the preferred choice for your most demanding applications.
Mechanical Plating & Galvanizing |
Electro- plating |
Hot-Dip & Dip-Spin Plating |
|
---|---|---|---|
No Hydrogen Embrittlement / High Strength Part (145ksi+) | ✓ | ✗ | ✗ |
No Hydrogen Embrittlement / Hardened Parts (32 HRC+) | ✓ | ✗ | ✗ |
Excellent Corrosion Protection (90-1000 hrs SST*) | ✓ | ✗ | ✓ |
Prevents Tempering of Hardened Parts | ✓ | ✓ | ✗ |
No Costly Post-Plating Baking Required | ✓ | ✗ | ✓ |
Uniform Coating Thickness on Complex Parts | ✓ | ✗ | ✗ |
Excellent Thread Fit | ✓ | ✓ | ✗ |
Eliminates Post-Plating Machining (e.g. threaded nuts) | ✓ | ✓ | ✗ |
Flat Parts Compatible (no sticking, nesting, or masking) | ✓ | ✗ | ✗ |
No Pitting | ✓ | ✗ | ✓ |
Stress-Free | ✓ | ✗ | ✗ |
No “Dog Bone” Thickness Distribution | ✓ | ✗ | ✗ |
Reduced Part Tangling (e.g. springs) | ✓ | ✗ | ✗ |
Excellent Adhesion Strength | ✓ | ✗ | ✓ |
No Blistering in Plating | ✓ | ✗ | ✗ |
Capable of Plating Sintered Parts Without Impregnation | ✓ | ✗ | ✗ |
Cost Effective on Thinner Coatings (<.00015 - .0003") | ✓ | ✓ | ✓ |
Cost Effective on Thicker Coatings (≥ .0005-.003″) | ✓ | ✗ | ✓ |
Appropriate for Parts ≤ 12″ in length and/or ≤ 1 pound | ✓ | ✓ | ✓ |
Non-Hazardous Disposal | ✓ | ✗ | ✗ |
*Salt spray testing. Higher noted values require a topcoat |